Main features:
1. The oxide layer on the surface shall be peeled according to different size requirements of the customer, and the surface finish shall reach Ra6.3.
2. The peeling thickness is even, the waste peel falls off and automatically rolls into complete waste, and the recovery rate can be increased by 20%-30%.
3. The peeling thickness can be 0.6mm-4mm on one side according to customer requirements.
4. High processing efficiency, whole process automation, time-saving and labor saving.
5. It is installed between the heating furnace and the extruder, without changing the original equipment.